Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Determination of Diffusion Layer Depth in Nitrided Layers: Testing Methods and Standards

Determination of the diffusion layer depth in nitrided steel components is essential for verifying case hardness profiles, fatigue performance, and heat-treatment process control in gas nitriding, plasma nitriding, and salt-bath nitrocarburizing. This technical article explains the metallographic and microhardness traverse methods used to measure the diffusion zone depth in accordance with GB/T 11354-2005, DIN 50190-3, ISO 6507-1, and ASTM E384. It also covers specimen preparation, testing items, typical industrial applications, and frequently asked questions relevant to metallurgical laboratories and heat-treatment quality engineers.

Technical Overview

Nitriding is a thermochemical surface-hardening process in which nitrogen is diffused into the surface of ferrous materials at temperatures typically between 500 °C and 590 °C, using gas nitriding, plasma (ion) nitriding, or salt-bath nitrocarburizing. The nitrided case consists of two metallurgically distinct regions: a thin compound layer (commonly called the white layer) composed of iron nitrides such as ε-Fe2–3N and γ′-Fe4N, and beneath it a substantially thicker diffusion zone in which nitrogen exists in interstitial solid solution and as extremely fine alloy-nitride precipitates such as CrN, AlN, VN, and molybdenum nitrides.

The diffusion zone is the principal contributor to the improved fatigue strength, load-bearing capacity, and wear reserve of nitrided components. Because hardness decreases gradually from the surface toward the unaffected core, the diffusion layer depth must be quantitatively determined to demonstrate conformance with drawing specifications, validate process parameters, and support failure analysis.

Several interrelated quantities are used in practice: the total nitrided case depth (compound layer plus diffusion zone), the diffusion layer depth itself, and the effective nitriding hardness depth (NHD), defined as the depth at which the hardness falls to a specified limit value, commonly the core hardness plus 50 HV. The authoritative procedures are given in GB/T 11354-2005 and DIN 50190-3, while hardness measurements are performed in accordance with ISO 6507-1, GB/T 4340.1, and ASTM E384.

Testing Samples

Metallographic Cross-Section Specimens

These are coupons sectioned perpendicular to the nitrided surface, with the treated surface fully preserved and free of rounding or chipping. Typical specimens are 10–20 mm in width with sufficient thickness to represent the part. For cylindrical parts such as shafts and rods, a full radial section is preferred so that the depth can be measured at the mid-radius position where curvature effects are minimal.

Sacrificial Sections from Actual Components

When verification must be performed on real parts, a representative location is cut from the component, for example a tooth section of a gear, a lug on a crankshaft counterweight, or a designated overrun area. The sampling location and measurement direction (flank, tip, root, or journal) must be documented because local depth can vary with geometry, gas flow, plasma density, and surface condition.

Companion (Witness) Coupons

For production control, witness coupons made from the same steel heat and surface condition are nitrided together with the workload in the same furnace charge. Coupon dimensions should be large enough that at least three times the expected case depth is available for core-hardness measurement. Testing witness coupons avoids destructive sectioning of deliverable parts and is widely accepted for routine batch release.

Testing Items

Accredited third-party laboratories and in-house metallurgical laboratories typically report the following items for a nitrided layer evaluation:

  • Diffusion zone depth, measured from the compound-layer boundary or from the original surface to the point where hardness or microstructure becomes indistinguishable from the core
  • Total nitrided case depth, comprising the compound layer plus the diffusion zone
  • Effective nitriding hardness depth (NHD), determined at the limit hardness of core hardness plus 50 HV per DIN 50190-3
  • Compound (white) layer thickness, including an assessment of porosity at the outer surface
  • Microhardness–depth profile, normally generated with HV0.1 to HV0.5 Vickers indentations
  • Surface (case) hardness and core hardness values
  • Microstructural evaluation, including nitride morphology, decarburization check, and surface brittleness rating per GB/T 11354

Testing Methods

Specimen Preparation

Reliable depth measurement begins with careful preparation. Sectioning must be performed under abundant coolant at low feed rates to avoid heating or mechanically damaging the brittle case. Specimens are mounted in resin with good edge retention; when preservation of the compound layer is critical, a thin electrolytic nickel plating of approximately 10–20 µm is applied before mounting to protect the outer edge. Grinding and polishing proceed through successive steps to a finish of 1 µm diamond or finer, ensuring that the surface layer is flat, unrounded, and free of smearing. Any edge rounding or relief will systematically shorten the measured depth.

Metallographic (Microscopic) Method

In the metallographic method, the polished cross section is etched to reveal nitrogen-affected regions. Etching with 2–4 % nital (nitric acid in ethanol) darkens the diffusion zone because of its fine nitride precipitates, while the compound layer remains largely white. A selenium-based etchant (selenic acid, hydrochloric acid, and ethanol), as referenced in GB/T 11354, selectively tints nitrogen-enriched zones a distinctive violet-blue color and provides clearer visualization of the diffusion-zone boundary.

The depth is measured at magnifications of 100× to 500× using a calibrated eyepiece scale or video measurement system. At least five to ten evenly distributed fields should be measured, and the arithmetic mean is reported to the nearest 0.01 mm. The main limitation of the method is subjectivity at the diffusion-zone boundary, particularly in steels whose core microstructure gives weak etching contrast; for this reason, the metallographic method is used for routine inspection and the microhardness method serves as the referee method.

Microhardness Traverse Method (Referee Method)

The microhardness method quantifies the diffusion layer through a hardness-depth curve. Vickers indentations are placed on a straight line perpendicular to the nitrided surface using a single test force, typically HV0.1 for shallow cases and HV0.5 for deeper cases, in accordance with ISO 6507-1, GB/T 4340.1, and ASTM E384. The center-to-center spacing between adjacent indentations, and between the first indentation and the specimen edge, must be at least 2.5 to 3 times the indentation diagonal to avoid mutual interaction. Typical traverse increments are 25–50 µm for shallow nitrocarburized cases and up to 100 µm for deep gas-nitrided cases.

Core hardness is established as the average of at least five indentations located well beyond the case, typically at depths greater than three times the expected case depth. The limit hardness is then calculated as the core hardness plus 50 HV. The effective depth is obtained by interpolation between the two adjacent indentations that bracket the limit hardness, and the result is reported to the nearest 0.01 mm together with the test force, indentation spacing, core hardness, and limit hardness. Knoop indentation, also covered by ASTM E384, can be used advantageously close to the surface because its elongated diagonal provides higher depth resolution.

When a compound layer is present, the traverse includes it; the report should therefore state clearly whether the depth datum is the original surface (total case) or the compound-layer boundary (diffusion zone only). Testing is performed with hardness testers verified and calibrated with reference blocks traceable to national standards, and repeated traverses on the same specimen are recommended to confirm repeatability.

Applications

Diffusion layer depth determination is applied across industries in which nitrided components carry fatigue, wear, or corrosion-duty requirements:

  • Automotive: crankshafts, camshafts, timing gears, valve stems and seats, and fuel-injection plungers and nozzle bodies
  • Aerospace and energy: actuator rods and cylinders, high-strength fasteners, and precision shafts subjected to high cycle fatigue
  • Tooling and die making: hot-work forging dies, plastic injection molds, extrusion tooling, and cold-forming punches
  • Fluid power and general machinery: hydraulic cylinder rods, piston rods, pump plungers, valve spools, spindles, and ball-screw shafts
  • Materials routinely evaluated: nitriding steels such as 41CrAlMo7 (38CrMoAl) and 31CrMoV9; quenched-and-tempered alloy steels such as 42CrMo4; hot-work and cold-work tool steels such as H13 and D2; and plasma-nitrided stainless steels

Beyond routine release testing, depth measurements support process qualification and requalification, incoming and outgoing inspection, comparison of gas versus plasma nitriding routes, root-cause investigation of premature wear or fatigue failures, and lifetime modeling based on the hardness gradient.

FAQ

What is the difference between the compound layer and the diffusion zone?

The compound layer is a thin, hard, brittle layer of iron nitrides, typically 5–30 µm thick, formed directly at the surface. The diffusion zone beneath it contains nitrogen dissolved in the matrix and ultra-fine alloy-nitride precipitates, typically 0.1–0.8 mm deep, and provides the major part of the fatigue and load-bearing improvement.

Which method is the referee method for diffusion layer depth?

The microhardness traverse method is recognized as the referee (arbitration) method under GB/T 11354-2005 and forms the basis of NHD determination in DIN 50190-3, because it is quantitative and less dependent on operator interpretation than metallographic etching.

What limit hardness criterion defines the effective depth?

The effective nitriding hardness depth is defined at the depth where the hardness falls to the core hardness plus 50 HV. The core hardness must be measured well beyond the nitrided case and averaged over several indentations.

What are typical achievable diffusion depths?

Gas and plasma nitriding of nitriding steels commonly produce diffusion zones of 0.2–0.7 mm after cycle times of 10–80 hours, while ferritic nitrocarburizing of unalloyed or low-alloy steels typically yields 0.1–0.3 mm. Because nitriding is performed below the transformation temperature, growth is slow and dimensionally stable, which is why depth verification is economically significant.

Can testing be performed on actual parts?

Yes, provided a sacrificial location can be sectioned. Where destructive sampling of deliverable parts is not acceptable, witness coupons nitrided in the same furnace charge are tested by accredited third-party laboratories under an agreed sampling plan.

Which test loads are used for the hardness traverse?

Loads between HV0.1 and HV0.5 are typical. Lower forces improve near-surface resolution but increase scatter, so the force is selected so that indentations remain measurable and the diagonal-based spacing rules of ISO 6507-1 and ASTM E384 can be respected.

Why Choose ZKGX?

  • State-of-the-art analytical equipment